RECYCLABLE BONDED AIR-LAID BLANKS

A method of producing a bonded air-laid blank (10) comprises introducing recycled cellulose and/or lignocellulose material and polymer binder fibers into a forming head (110). The recycled cellulose and/or lignocellulose material comprises at least 75 % by weight of cellulose and/or lignocellulose material flakes (30) having an average largest dimension selected within an interval of from 2 up to 20 mm. The polymer binder fibers have an average length of less than 17.5 mm. The method also comprises capturing the recycled cellulose and/or lignocellulose material and the polymer binder fibers as an unbonded air-laid web (20) on a conveyor (120) arranged in connection with an outlet (113) of the forming head (110), and heating the unbonded air-laid web (20) to at least partly melt the polymer binder fibers and bind the recycled cellulose and/or lignocellulose material to form a bonded air-laid blank (10) comprising less than 10 % by weight of the polymer binder fibers and at least 80 % by weight of the recycled cellulose and/or lignocellulose material.

申请(专利)号 SE2430673A
申请日期 2024年12月19日
公开(公告)日 2026年9月2日
公开(公告)号 SE548484C2
主分类号 D04H1/732
分类号 D04H1/732 B27N3/04 D04H1/26 D21B1/08 D21H11/14
申请(专利权)人 Stora Enso Oyj
发明(设计)人 Malmqvist, Martin Persson, Lars