军事知识服务平台
NiW涂层热震性能与挥发性能研究
Thermal Shock Performance and Volatilization Performance of NiW Coatings
摘要 针对镍基合金在高温高真空环境下服役时易发生元素挥发的瓶颈问题,采用脉冲直流磁控溅射技术在合金表面制备 NiW 涂层,系统考察了其热震性能与挥发性能.通过800℃热震实验评估涂层的结合力演变,并结合900℃高温挥发实验研究其长效防护行为.利用 XRD、SEM、EDS 分析了涂层的物相、形貌及元素分布,采用纳米划痕仪表征界面结合强度,并通过高精度质量损失测量计算挥发速率.结果表明:经800℃热震后,涂层发生相结构转变,hcp-NiW 相消失,晶粒发生粗化;热震结束后涂层与基体的结合力较沉积态显著提升11.10 N,表现出良好的热机械稳定性.在900℃挥发实验后,hcp-NiW 相消失,涂层内产生了新相.元素分析表明,挥发过程中 W元素在表层逐渐富集,而 Ni、Cr 元素含量持续降低,W 富集层的形成有效抑制了基体元素的进一步挥发.挥发速率呈现先升高后降低的趋势,初始阶段最慢,为 1.213×10-8 mg/(mm2·h).由此可见,NiW 涂层的抗挥发性能并非仅由W 含量单一因素决定,而是扩散通道与阻挡层协调作用的结果.在长期服役中,促进连续致密的W 层的快速形成、同时抑制扩散通道的过度连通,是提升涂层挥发寿命的关键.
Abstract:
With the continuous advancement of space exploration missions,space nuclear reactor power systems have become key energy sys-tems because of their high power density and long service life.However,heat pipes,as one of the core components of nuclear reactors,are ex-posed to long-term high-temperature(770℃)and high-vacuum environments,under which material volatilization becomes significant and may readily lead to performance degradation or even failure.Therefore,the development of protective coatings with excellent resistance to volat-ilization is of great importance.NiW coatings show promising resistance to volatilization owing to the high melting point and low saturated vapor pressure of tungsten(W),as well as the compositional transition effect provided by nickel(Ni)between the substrate and the coating. In this study,NiW coatings were prepared on a nickel-based superalloy substrate by pulsed direct-current magnetron sputtering,and their thermal shock stability and resistance to volatilization were systematically investigated.The service performance of the coatings was evaluated through thermal shock and high-temperature volatilization tests.The thermal shock tests were conducted for 30 cycles at 800℃under 3×10-3 Pa,while the volatilization tests were performed at 900℃under 1×10-4 Pa for 720 h.The phase structure,microstructure,and elemental dis-tribution of the coatings were characterized by X-ray diffraction(XRD),scanning electron microscopy(SEM),and energy-dispersive spec-troscopy(EDS),respectively.Interfacial adhesion strength was evaluated by nanoscratch testing,and the volatilization rate was calculated based on mass loss. The results showed that significant phase transformation and grain coarsening occurred during thermal shock.The hcp-NiW phase disap-peared,and obvious evolution was observed in the surface and cross-sectional microstructures as well as in the elemental distribution.Mean-while,after thermal shock,the interfacial adhesion strength between the coating and the substrate increased by approximately 11.10 N com-pared with that of the as-deposited coating,indicating that the coating retained good mechanical stability under cyclic thermal loading.After holding at 900℃for 720 h,the hcp-NiW phase completely disappeared and new phases formed.During volatilization,W gradually became enriched at the surface,whereas Ni and Cr continuously diffused outward and volatilized,resulting in the formation of a W-enriched layer that effectively suppressed further elemental volatilization.The volatilization rate first increased and then decreased with time.This behavior was at-tributed to the possible formation of interconnected diffusion pathways within the coating during the intermediate stage of volatilization,which accelerated the outward diffusion and volatilization of Ni and Cr.During the later stage,however,depletion of Cr and Ni together with the for-mation of a continuous and dense W layer effectively hindered the migration of the remaining elements.The temporal mismatch between these two processes resulted in the overall trend of an initial increase followed by a decrease in the volatilization rate.In addition,the lowest volatili-zation rate,1.213×10-8 mg/(mm2·h),was observed at the initial stage,indicating that the rapid formation of a stable diffusion barrier is crucial for reducing long-term mass loss. The resistance to volatilization of NiW coatings is governed by the synergistic effects of diffusion-pathway evolution and the formation of a dense W-enriched layer,rather than solely by W content.During long-term service,promoting the rapid formation of a continuous and dense W layer while suppressing excessive interconnection of diffusion pathways is key to improving the volatilization resistance and service life of the coatings.This study provides important theoretical and experimental support for the design of heat-pipe materials for space nuclear reactors and has important engineering significance for the development of protective materials used in extreme environments.
刊 名 材料保护 ISTIC
年,卷(期): 2026, 59(10)
分类号: TG174
机标分类号: TG139.6 TN304.055 TB383
在线出版日期: 2026年11月11日