Inhibitory Effect of Current Collectors on the Self-Discharge Performance of Aqueous Zinc-Ion Batteries
摘要
为填补负极集流体与水系锌离子电池自放电关联的实验研究空白,厘清集流体诱发副反应造成容量衰减的核心机理,创新性地从实验层面探究水系锌离子电池(AZIBs)负极集流体对自放电性能的影响规律,以二氧化锰(MnO2)为正极活性物质、锌粉为负极活性物质,分别采用镀锡铜网与铜箔作为负极集流体,构建 AZIBs 体系.通过扫描电子显微镜(SEM)、X 射线衍射仪(XRD)、X 射线光电子能谱(XPS)等表征方法和恒流充放电、开路电压(OCV)监测、线性扫描伏安法(LSV)、电化学阻抗谱(EIS)等测试方法,分别从材料结构和电性能角度研究了 2 种集流体对电池自放电性能的影响及作用机制.结果表明,在 100%荷电状态(SOC)条件下静置 7 d,铜箔集流体电池的开路电压日均衰减速率为 13.71 mV/d,相较于镀锡铜网体系的 16.14 mV/d 降幅约 15%;铜箔优异的化学稳定性及二维平面结构可减少锌负极与电解液的副反应,抑制锌的枝晶生长与腐蚀溶解,电池循环寿命大于 500圈,明显高于镀锡铜网体系.本研究为 AZIBs 负极集流体设计,提升电池储存稳定性提供关键实验依据,对推动AZIBs 在储能领域的产业化应用具有重要意义.
To fill the experimental research gap concerning the relationship between negative current collectors and self-discharge in aqueous zinc-ion batteries(AZIBs),and to clarify the core mechanism by which current-collector-induced side reactions cause capacity decay,the in-fluences of negative current collectors on the self-discharge performance of AZIBs were systematically investigated at the experimental level.AZIBs were assembled using manganese dioxide(MnO2)as the cathode active material,zinc powder as the anode active material,and either tin-plated copper mesh or copper foil as the negative current collector.Scanning electron microscopy(SEM),X-ray diffraction(XRD),and X-ray photoelectron spectroscopy(XPS)were used for structural characterization.Galvanostatic charge-discharge testing,open-circuit voltage(OCV)monitoring,linear sweep voltammetry(LSV),and electrochemical impedance spectroscopy(EIS)were used to examine the effects of the two current collectors on cell self-discharge and the underlying mechanism from the perspectives of material structure and electrochemical performance.The results showed that after storage for 7 d at 100%state of charge(SOC),the mean daily open-circuit voltage decay rate of the cell with a copper-foil current collector was 13.71 mV/d,approximately 15%lower than the 16.14 mV/d measured for the tin-plated copper mesh system.The superior chemical stability and two-dimensional planar structure of the copper foil reduced side reactions between the zinc an-ode and the electrolyte,and inhibited zinc dendrite growth and corrosion dissolution.The cell with the copper-foil current collector exhibited a cycle life of more than 500 cycles,markedly longer than that of the tin-plated copper mesh system.This study provided key experimental evi-dence for the design of negative current collectors for AZIBs and for improving battery storage stability.It was also of great significance for pro-moting the industrial application of AZIBs in energy storage.