摘要
探讨了基底温度(25~200℃)对常压等离子体射流制备类 SiO2 薄膜的影响.在高温下沉积的薄膜厚度有所减小(从242 nm 降至156 nm),但机械和化学性能得到增强,铅笔硬度从B 提高到4H.基底温度不低于100℃时制备的薄膜附着力提高到0 级(无脱落).X 射线光电子能谱证实,基底温度从 25℃升至200℃,所制得的薄膜的碳含量减少,SiO2 含量增加,表明前驱体分解加剧.盐酸腐蚀测试(浸渍 3.0 h)表明,基底温度为200℃时制备的薄膜耐腐蚀性增强,质量损失6.53%,而无涂层对照组质量损失7.01%.结果表明,基底温度是制备应用于腐蚀性环境中的防护涂层的关键工艺参数.
This study explores the effects of the substrate temperature(25-200℃)on SiO2-like thin films prepared via atmospheric-pressure plasma jet.Films deposited at elevated temperatures exhibited a reduced thickness(from 242 to 156 nm)but enhanced mechanical and chemical performance.The pencil hardness improved from grade B to 4H.The adhesion reached class 0(no detachment)at temperatures of 100℃and above.X-ray photoelectron spectroscopy(XPS)confirmed carbon reduction and silicon dioxide(SiO2)enrichment when the substrate temperature increased from 25 to 200℃,indicating intensified precursor decomposition.Hydrochloric acid corrosion testing(3.0 h immersion)revealed that the films deposited at 200℃exhibited improved corrosion resistance,with a mass loss of 6.53%compared to 7.01%for the bare substrates.The results indicate that the substrate temperature is a critical process parameter for preparing protective films applied in corrosive environments.