The effect of hydrothermal temperature on the electrochromic properties of nickel oxide thin films
摘要
水热温度是水热法制备NiO薄膜的一个重要参数.利用NiCl2·6H2O与CO(NH2)2作为反应前驱体溶液,分别以140、150、160和170 ℃的水热温度进行50 min水热反应,探究水热温度对NiO薄膜形貌及电致变色性能的影响.利用场发射扫描电子显微镜(FE-SEM)、电化学工作站和紫外-可见分光光度计对薄膜进行形貌表征与性能测试.NiO膜厚随着水热温度的升高先增加后减小;薄膜呈现纳米片结构,升高至170 ℃时薄膜出现不规则聚集体纳米花结构.当水热温度为160 ℃时,NiO薄膜最厚,大约370 nm,薄膜具有较大比表面积,能够提供更多活性位点,储存更多电荷,加快离子注入与脱出.因此该NiO薄膜具有较高电荷容量(24.91 mC/cm2),更快的响应时间(致色时间6.2 s,褪色时间2.9 s).在波长600 nm处的光调制幅度为50.56%,其光密度变化与致色效率分别为 0.42 和 17 cm2/C.
Hydrothermal temperature is a crucial parameter for the preparation of NiO thin films.NiCl2·6H2O and CO(NH2)2 were used as precursor solution,and hydrothermal reactions were conducted at 140,150,160 and 170℃ for 50 min.The effect of hydrothermal temperatures on the morphologies and electrochromic per-formance of NiO thin films were investigated.The morphologies and performances of the thin films were char-acterized and tested using a field emission scanning electron microscope(FE-SEM),an electrochemical worksta-tion and a UV-visible spectrophotometer.The thickness of NiO thin films increased and then decreased with the hydrothermal temperatures.Thin films exhibit nanoflake-structure.When the temperature rose to 170℃,the thin film presents an irregular aggregated nanoflower structure.As the hydrothermal temperature is 160℃,the NiO film is the thickest about 370 nm with a large specific surface area,which can offer more active sites,store more charge and accelerate ion implantation and extraction.Therefor this NiO film has a higher charge capacity(24.91 mC/cm2)and a faster response time(coloring time 6.2 s and bleaching time 2.9 s).The optical modula-tion amplitude is 50.56%at the wavelength of 600 nm.The optical density change and coloration efficiency are 0.42 and 17 cm2/C,respectively.