Effect of tempering treatment on the microstructure and impact-corrosion-wear behavior of high chromium cast iron
摘要
以高铬铸铁为研究对象,开展不同温度回火处理,结合OM、SEM、EDS等微观表征与硬度、冲击韧性、冲击-腐蚀-磨损等性能测试,研究回火温度对其显微组织、力学性能及冲击-腐蚀-磨损行为的影响.结果表明,回火后高铬铸铁组织主要由共晶碳化物、回火马氏体及二次碳化物构成.随着回火温度升高,网状共晶碳化物发生重组,基体针状马氏体特征减弱,并逐步向回火屈氏体、回火索氏体转变;低温回火(≤320℃)下材料硬度(HRC)维持在60以上,550 ℃高温回火后硬度(HRC)大幅降至48.09;回火温度对冲击韧性影响较小,材料整体仍呈脆性断裂特征.在低于450 ℃回火时,不同冲击载荷下的质量损失率均稳定保持在21.6~26.2 mg/h范围,当回火温度升高至550 ℃,质量损失率显著增大至34.8~38.4 mg/h,抗冲击-腐蚀-磨损性能急剧恶化.
In this study,high chromium cast iron was subjected to tempering treatment at different tem-peratures.The effects of tempering temperature on its microstructure,mechanical properties,and im-pact corrosion-wear behavior were investigated using OM,SEM,EDS,as well as property tests of hard-ness,impact toughness and impact-corrosion-wear tests.The results show that the tempered microstruc-ture of high chromium cast iron mainly consists of eutectic carbides,tempered martensite,and second-ary carbides.As the tempering temperature increases,the network eutectic carbides undergo reorganiza-tion,the characteristic of acicular martensite in the matrix weakens,and the matrix gradually transforms into tempered troostite and tempered sorbite.After low-temperature tempering(≤320 ℃),the hardness(HRC)remains above 60,whereas after high-temperature tempering at 550 ℃,the hardness(HRC)significantly decreases to 48.09.The tempering temperature has a minor effect on im-pact toughness,and the material still exhibits predominantly brittle fracture characteristics.When tempered below 450℃,the mass loss rate under different impact loads remains stable within the range of 21.6-26.2 mg/h.However,when the tempering temperature rises to 550℃,the mass loss rate signi-ficantly increases to 34.8-38.4 mg/h,indicating a sharp deterioration in the impact-corrosion-wear resist-ance.