摘要
为了研究冷轧预变形对TWIP钢氢脆行为的影响,以10%和20%冷轧预变形TWIP钢为研究对象,采用慢应变速率拉伸、疲劳裂纹扩展、热脱附分析和微观组织表征等方法,研究该材料的氢脆损伤行为.结果表明,冷轧变形显著提高TWIP钢的强度并降低其塑性,20%冷轧后屈服强度由325 Mpa提高至1 067 Mpa,延伸率由64.8%降至21.3%;随着冷轧变形量增加,试样的氢含量和氢扩散系数均升高,在5 Mpa H2环境下,各试样的塑性损失较小,热充氢后氢脆敏感性明显增加,其中 20%冷轧试样的相对延伸率和相对断面收缩率分别降至 71.6%和74.6%,断口呈现更明显的准解理特征.冷轧预变形在N2和H2环境下均降低了疲劳裂纹扩展速率,但与N2环境相比,H2环境促进了疲劳裂纹扩展.预变形孪晶在裂纹扩展前期通过阻碍位错运动抑制氢致裂纹扩展;随着裂纹扩展,氢在孪晶界附近富集并促进沿孪晶界开裂,使其抑制作用逐渐减弱.
To investigate the effect of cold rolling pre-deformation on hydrogen embrittlement behavior in TWIP steel,10%and 20%cold rolling pre-deformed TWIP steel were studied using slow strain rate tensile tests,fatigue crack growth tests,thermal desorption analysis,and microstructural characterization to examine the hydrogen embrittlement damage behavior of the material.Results showed that no martensitic transformation was detected during cold rolling pre-deformation or subsequent deformation under hydrogen-containing conditions.Cold rolling significantly increased the strength of the TWIP steel while reducing its ductility.After 20%cold rolling,the yield strength increased from 325 MPa to 1,067 MPa,whereas the elongation decreased from 64.8%to 21.3%.Both the hydrogen content and hydrogen diffusion coefficient increased with increasing cold rolling reduction.In a 5 MPa H₂ environment,all specimens exhibited relatively small ductility losses.After thermal hydrogen charging,the susceptibility to hydrogen embrittlement increased markedly.The relative elongation and relative reduction in area of the 20%cold rolling specimen decreased to 71.6%and 74.6%,respectively,accompanied by more pronounced quasi-cleavage fracture features.Cold rolling pre-deformation reduced the fatigue crack growth rates in both N2 and H2 environments,whereas the H2 environment accelerated fatigue crack growth.Pre-existing deformation twins suppressed hydrogen-assisted crack growth at the early stage of crack propagation by impeding dislocation motion.As crack propagation proceeded,hydrogen accumulation near twin boundaries promoted cracking along twin boundaries gradually weakened this suppressing effect.