10CrNiCu和10Ni8CrMoV钢动态剪切性能及微观组织分析
Dynamic Shear Properties and Microstructure Analysis of 10CrNiCu Steel and 10Ni8CrMoV Steel
摘要 为探究10CrNiCu钢与10Ni8CrMoV钢在动态剪切载荷下的力学性能差异及微观组织变化规律,采用分离式霍普金森压杆(SHPB)试验系统对其分别在1 500 s-1、2 500 s-1、4 000 s-1应变率下进行动态剪切试验,通过金相组织观察、显微硬度测试、扫描电子显微形貌表征,分析了应变率对两种钢材剪切力学曲线、绝热剪切带形貌及微观组织演化的影响规律.试验结果表明,两种钢材均呈现显著的应变率强化效应,在高应变率下均会生成绝热剪切带;10CrNiCu钢剪切带组织转变为贝氏体,剪切带中心硬度较基体提升40%,高应变率下无剪切裂纹萌生,结构稳定性优异;10Ni8CrMoV钢剪切带形成细小板条马氏体,硬度提升36%,但当剪应变率≥2 500 s-1 时,10Ni8CrMoV钢易产生微裂纹并发生剪切失效.综合对比可知,10CrNiCu钢的抗动态剪切性能更优.
Abstract:
To investigate differences in mechanical properties and the evolution of microstructure under dynamic shear loading between 10CrNiCu steel and 10Ni8CrMoV steel,dynamic shear tests were conducted at strain rates of 1 500 s-1、2 500 s-1、4 000 s-1 using the Split Hopkinson Pressure Bar(SHPB)test system.The influence of strain rate on the shear stress-strain curves,adiabatic shear band morphology,and microstructural evolution of the two steels was analyzed by metallographic observation,microhardness testing,and scanning electron microscopy(SEM)characterization.Results indicate that both steels exhibit significant strain rate strengthing effects and form adiabatic shear bands under high strain rate loading.For 10CrNiCu steel,the shear band transforms into bainite,with a hardness increase of 40%at the center of the shear band compared to the matrix.No shear cracks initiate under high strain rates,demonstrating excellent structural stability.The shear band of 10Ni8CrMoV steel transformed into fine lath martensite,and the hardness increased by about 36%,but the dynamic shear failure occurred at the strain rate of 2 500 s-1 and above.Comprehensive comparison reveals that 10CrNiCu steel exhibits superior resistance to dynamic shear.
刊 名 焊管
年,卷(期): 2026, 49(9)
分类号: TG142.33
机标分类号: TG142.1 U4 O347.3
在线出版日期: 2026年10月14日