军事知识服务平台
某含钛铁精矿工艺矿物学及提质试验研究
Study on the Process Mineralogy and Quality Improvement Test of a Titanium-Bearing Iron Concentrate
摘要 为进一步提升攀西地区某含钛铁精矿的铁品位,开展了工艺矿物学与细磨—磁选试验研究.通过矿物嵌布特征与元素赋存状态分析,明确了影响精矿提质的矿物学因素,并评估了细磨提质的可行性.结果表明,样品TFe品位为41.59%,TiO2含量为10.84%;主要有用矿物为钛磁铁矿和钛铁矿,脉石以辉石、绿泥石、钛闪石、角闪石和斜长石为主.铁主要赋存于磁性铁矿物中,分布率为90.12%;钛主要分布于钛磁铁矿和钛铁矿中,其中钛磁铁矿中TiO2分布率为65.59%.钛磁铁矿、钛铁矿和榍石均以细粒嵌布为主,且与脉石连生紧密,钛磁铁矿单体解离度仅为36.12%,是限制铁精矿品位提升的主要因素.采用卧式搅拌磨将物料磨至-45μm占比90%后,矿物解离度显著改善;经两段磁选,最终获得产率78.06%、TFe品位50.90%、TFe回收率95.54%的磁选精矿,精矿中SiO2、MgO、Al2O3和CaO等脉石组分明显降低.结果表明,细磨—多段磁选工艺可有效实现钛磁铁矿精矿的提质降杂,研究结果为攀西地区钒钛磁铁矿精矿的深度提质提供了技术参考.
Abstract:
To further improve the iron grade of a titanium-bearing iron concentrate in the Panxi area,a process mineralo-gy and fine grinding-magnetic separation experimental study was conducted.Through analysis of mineral dissemination charac-teristics and element occurrence states,the mineralogical factors affecting concentrate upgrading were clarified,and the feasibil-ity of fine grinding for upgrading was evaluated.The results show that the sample has a TFe grade of 41.59% and a TiO2 con-tent of 10.84%.The main valuable minerals are titanomagnetite and ilmenite,while the gangue minerals are mainly pyroxene,chlorite,kaersutite,hornblende,and plagioclase.Iron is mainly hosted in magnetic iron minerals,with a distribution rate of 90.12%;Titanium is mainly distributed in titanomagnetite and ilmenite,among which the TiO2 distribution rate in titanomagne-tite is 65.59%.Titanomagnetite,ilmenite,and sphene are mainly finely disseminated and closely intergrown with gangue miner-als.The liberation degree of titanomagnetite is only 36.12%,which is the main factor limiting the improvement of iron concen-trate grade.After grinding the material to 90% passing 45 μm using a horizontal stirred mill,the mineral liberation was signifi-cantly improved.Through two-stage magnetic separation,a magnetic concentrate with a yield of 78.06%,Tfe grade of 50.90%,and Tfe recovery of 95.54% was obtained,and the contents of gangue components such as SiO2,MgO,Al2O3,and CaO in the concentrate were significantly reduced.The results indicate that the fine grinding and multi-stage magnetic separa-tion process can effectively upgrade and reduce impurities in titanomagnetite concentrate.This study provides a technical refer-ence for the deep upgrading of vanadium-titanium magnetite concentrate in the Panxi area.
刊 名 金属矿山 ISTICPKU
年,卷(期): 2026, (9)
分类号: TD951 TD913
机标分类号: TD951 P575 P618
在线出版日期: 2026年10月9日
基金项目: 52174243:国家自然科学基金2024JH2/102400026:辽宁省重点研发计划项目,