Cause analysis and improvement of oxide scale in hot-rolled dual-phase steel
摘要 针对1 780 mm热连轧生产线HC340/590DP双相钢热轧卷存在的表面氧化铁皮缺陷问题,对热连轧带钢表面氧化铁皮的形成机理进行系统研究,深入探讨了加热炉在炉时间、高温段停留时间以及除鳞压力等关键工艺参数对钢材表面质量的影响规律.生产实践表明:通过采取缩短在炉时间、减少精轧时间以及提高粗除鳞压力等工艺优化措施,能够有效抑制氧化铁皮缺陷的产生,显著改善带钢的表面质量.
Abstract:
Aiming at the surface oxide scale defect in hot-rolled coils of HC340/590DP dual-phase steel produced on 1 780 mm hot continuous rolling line,formation mechanism of oxide scale on surface of hot-rolled strip steel is systematically in-vestigated,detailed study was conducted on influence patterns of key process parameters such as furnace residence time,holding time in high temperature section,and descaling pressure on surface quality of steel.Production practice shows that by implementing process optimization measures,including reducing furnace residence time,shortening finishing rolling time,and increasing rough descaling pressure,generation of oxide scale defects can be effectively suppressed,and surface quality of strip steel can be significantly improved.
刊 名 金属制品
年,卷(期): 2026, 52(4)
分类号: TG335.5
机标分类号: TG333 TH137 R47
在线出版日期: 2026年9月7日