为了探究SWRH82A热轧盘条在不同冷却速率下的组织转变规律,对样品进行不同冷却速率下的相变点温度测定、金相组织和硬度分析,根据测试结果绘制SWRH82A热轧盘条的连续冷却转变曲线.结果表明:相变点4c1=724.4℃,Accm=750.5 ℃,Ms=247.9 ℃.开始产生马氏体的临界冷却速率为15.0 ℃/s,冷却速率为0.5~10.0℃/s时组织主要为索氏体及少量珠光体、铁素体;冷却速率为15.0~35.0 ℃/s时,组织主要为索氏体和马氏体.经过工艺调整,控制相变前冷却速率在10.0 ℃/s,热轧盘条索氏体化率不低于85%,珠光体晶粒度≥7.5级,珠光体片层间距≤0.087 μm,抗拉强度不低于1 135 MPa.
To investigate microstructure transformation rules of SWRH82A hot-rolled wire rods under different cooling rates,phase transformation point temperatures,microstructures,and hardness values of samples were measured and analyzed under va-rious cooling rates.Based on test results,continuous cooling transformation curve of SWRH82A hot-rolled wire rods was plot-ted.Results indicate that phase transformation points are Ac1=724.4 ℃,Accm=750.5 ℃,and Ms=247.9℃.The critical cooling rate at which martensite begins to form is 15.0 ℃/s.When cooling rate ranges from 0.5 to 10.0℃/s,microstructure primarily consists of sorbite with minor pearlite and ferrite.When cooling rate ranges from 15.0 to 35.0 ℃/s,microstructure is predominantly composed of sorbite and martensite.After process adjustment,cooling rate before phase transformation is controlled at 10.0℃/s,sorbitization rate of hot-rolled wire rod is not less than 85%,pearlite grain size grade is not less than 7.5 grade,pearlite lamellar spacing is not more than 0.087 μm,and tensile strength is not lower than 1 135 MPa.