铝合金因其低密度、高比强度等特性在航空和海洋工程领域广泛应用,但硬度低、耐磨及耐腐蚀性能差等问题限制了其在严酷环境下的应用.针对2024铝合金在严酷海洋环境下的防护需求,在其表面构建了类金刚石(DLC)保护涂层.重点探讨了脉冲宽度对膜层微观组织演化、机械强度及电化学稳定性的影响规律.结果表明,脉冲宽度的波动主要通过改变sp2杂化键的畸变程度来影响薄膜的性能,而对于sp3杂化键含量的影响有限.在15μs脉冲宽度下,薄膜表现出最优的综合性能,其腐蚀电流密度最低,为3.16×10-7 A/cm2,表现出最佳的耐腐蚀性能.此外,该工艺参数下的薄膜硬度和弹性模量略高,与基体保持了良好的结合强度.
Aluminum alloys are widely used in aerospace and marine engineering due to their low density and high specific strength,but its low hardness and inadequate resistance to wear and corrosion limit their performance in aggressive environ-ments.To meet the protection requirements of 2024 aluminum alloy in harsh marine environments,diamond-like carbon(DLC)protective coating was developed on its surface.The primary focus is on evaluating the influence of pulse width on the microstructural evolution,mechanical properties,and electrochemical stability of the resulting coatings.Experimental results demonstrate that variations in pulse width predominantly affect coating characteristics by modifying distortion level of sp2 hybridized bonds,while exerting limited influence on the content of sp3 hybridized bonds.Optimal overall performance was achieved at pulse width 15 μs,where coating exhibited the lowest corrosion current density of 3.16 × 10-7 A/cm2,in-dicating superior corrosion resistance.Moreover,coatings deposited under this condition also showed slightly enhanced hardness and elastic modulus,along with excellent adhesion to substrate.
年,卷(期):
2026, 52(4)
分类号:
TG174.4
机标分类号:
TG146.21
TG306
TB383
在线出版日期:
2026年9月7日