摘要 金川镍渣主要来自硫化镍矿火法冶炼过程,属于典型富铁冶金渣,全铁含量高达30%~40%,并富含硅、钙、镁等有价组分,具有较高的资源回收潜力.本文通过熔融氧化法对镍渣进行高温矿相重构,使渣中铁由橄榄石相转变为磁铁矿相富集,继而通过磁选分离提取磁铁矿晶体.系统研究了氧化钙与二氧化硅含量变化对氧化镍渣中磁铁矿析晶行为、形貌结构及磁性能的影响机理.并结合X射线衍射(XRD)、扫描电子显微镜-能谱分析(SEM-EDS)与振动样品磁强计(VSM)等手段,揭示了不同组元在析晶过程中的作用机制.结果表明,随二氧化硅含量增加,磁铁矿衍射主峰向高角度方向偏移,表明硅离子部分取代铁离子.相较之下,氧化钙增加未引起明显峰位偏移,表明钙离子难以固溶于磁铁矿晶格.显微形貌与成分分析表明,二氧化硅增加导致体系黏度升高、磁铁矿颗粒细化.硅主要富集于辉石相,仅少量进入磁铁矿晶格;而钙主要分布于基体硅酸盐相中.磁性能方面,饱和磁化强度随二氧化硅含量呈先升高后降低的变化规律,在二氧化硅含量为32%(质量分数)时达最大值35.21 emu·g-1,表明适量二氧化硅有利于晶粒生长与磁畴有序排列,从而提升饱和磁化强度.当二氧化硅过量时,一方面,非磁性硅掺杂降低了磁铁矿的磁矩;另一方面,黏度升高导致颗粒过度细化以及非磁性的硅酸盐相包裹在磁铁矿颗粒中导致饱和磁化强度下降.氧化钙含量增加则导致磁铁矿晶粒长大、磁矩取向随机化,从而削弱整体磁化强度.综上,通过合理调控二氧化硅与氧化钙含量,可实现镍渣中磁铁矿的定向析出与磁性优化,为富铁镍渣铁资源的高值回收提供了成分设计与工艺优化依据.
Abstract:
Jinchuan nickel slag,generated primarily during the pyrometallurgical processing of sulfide nickel ores,is a typical iron-rich metallurgical residue with a total iron content of 30%-40%and abundant valuable components such as Si,Ca,and Mg,indicating substantial potential for resource recovery.In this study,high-temperature phase reconstruction was achieved via molten oxidation,whereby iron in the slag was transformed from olivine-associated phases to magnetite-enriched phases,followed by magnetic separation to recover magnetite crystals.The effects and mechanisms of varying CaO and SiO2 content on the crystallization behavior,morphology,and magnetic properties of magnetite in the oxidized nickel slag were systematically investigated.Phase evolution was characterized by X-ray diffraction,while microstructure and elemental partitioning were examined using scanning electron microscopy coupled with energy-dispersive spectroscopy;magnetic properties were evaluated using a vibrating sample magnetometer.The results show that increasing the SiO2 content shifts the main magnetite diffraction peak toward higher angles,suggesting partial substitution of Fe with Si within the magnetite lattice.By contrast,increasing CaO causes no pronounced peak shift,indicating that Ca has limited solubility in the magnetite structure.Microscopic and compositional analyses reveal that higher SiO2 increases melt viscosity and refines magnetite particles.Silicon is predominantly enriched in pyroxene phases,with only a small fraction incorporated into the magnetite lattice,whereas calcium mainly distributes in the silicate matrix.Magnetically,the saturation magnetization exhibits a non-monotonic dependence on SiO2 content,first increasing and then decreasing,and reaches a maximum of 35.21 emu·g-1at 32%SiO2.This indicates that an appropriate SiO2 level promotes grain growth and magnetic-domain ordering,thereby enhancing the saturation magnetization.When SiO2 is excessive,the saturation magnetization decreases due to(ⅰ)dilution of the magnetite magnetic moment by non-magnetic Si incorporation and(ⅱ)viscosity-induced over-refinement and encapsulation of magnetite particles by non-magnetic silicate phases.In contrast,increasing CaO leads to coarsening of magnetite grains and a more randomized magnetic-moment orientation,which weakens the overall magnetization.Overall,rational regulation of SiO2 and CaO contents enables controlled precipitation of magnetite and optimization of magnetic properties in nickel slag,providing a basis for compositional design and process optimization toward high-value recovery of iron resources from iron-rich nickel slags.
刊 名 矿冶 ISTIC
年,卷(期): 2026, 35(4)
分类号: TF09
机标分类号: TQ171.733 O643.36 R318.08
在线出版日期: 2026年9月15日
基金项目: 23JRRC0018:甘肃省科技计划联合科研基金重点项目2024GY009z:重点科技计划-工业类项目,