摘要
随着优质铁矿资源的日益枯竭,实现褐铁矿的高效利用对钢铁工业的可持续发展至关重要.本文系统综述了褐铁矿在球团工艺中的应用研究进展.褐铁矿(理论铁品位54.67%~62.68%)因其高结晶水含量及疏松多孔的蜂窝状结构,在焙烧过程中易导致球团爆裂,并阻碍赤铁矿晶桥充分连接,从而影响球团强度.针对这一技术瓶颈,现有研究主要围绕两方面展开:一是配矿优化方面,将褐铁矿与磁铁矿精矿按25%~33%的比例混合,利用褐铁矿比表面积大(1 800~2 200 cm2•g-1)的特性提升生球强度,并通过磁铁矿氧化放热补偿褐铁矿脱水热耗,以优化球团矿固结效果;但当褐铁矿配比超过30%时,球团抗压强度因孔隙率增加而显著下降.二是功能替代方面,利用超细磨褐铁矿作为含铁黏结剂替代50%~70%的膨润土,可使球团铁品位提升0.8~1.2个百分点,并降低高炉渣量15~30 kg·t-1.研究表明,当含铁黏结剂配比为4%时,球团抗压强度达到峰值2 785.7 N• P-1,同时还原膨胀率由19.69%显著降低至7.51%.结果可为球团工艺合理、高效利用褐铁矿提供参考.
With the increasing depletion of high-quality iron ore resources,the efficient utilization of limonite is crucial to the sustainable development of the steel industry.This paper systematically reviews the research progress on the application of limonite in pelletizing processes.Limonite(theoretical iron grade of 54.67%-62.68%),characterized by its high crystal water content and loose,porous honeycomb structure,is prone to pellet cracking during roasting and hinders the sufficient connection of hematite crystal bridges,thereby affecting pellet strength.To address this technical bottleneck,existing studies have mainly focused on two aspects.The first is ore blending optimization,in which limonite is mixed with magnetite concentrate at a ratio of 25%-33%.The high specific surface area of limonite(1 800-2 200 cm2•g-1)is utilized to improve green pellet strength,while the exothermic oxidation of magnetite compensates for the heat consumption of limonite dehydration,thereby optimizing the consolidation effect of pellets.However,when the limonite proportion exceeds 30%,the pellet compressive strength decreases significantly due to increased porosity.The second aspect is functional substitution,in which ultrafine-ground limonite is used as an iron-bearing binder to replace 50%-70%of bentonite.This can increase the iron grade of pellets by 0.8-1.2 percentage points and reduce blast furnace slag rate by 15-30 kg·t-1.Studies have shown that when the iron-bearing binder addition is 4%,the pellet compressive strength reaches a peak value of 2 785.7 N·P-1,while the reduction swelling index decreases significantly from 19.69%to 7.51%.This review can provide reference for the rational and efficient utilization of limonite in pelletizing operations.