焦磷酸哌嗪合成及阻燃聚丙烯研究
Research on synthesis of piperazine pyrophosphate and its application in flame-retardant polypropylene
摘要 以磷酸和哌嗪为原料通过两步法制备焦磷酸哌嗪(PAPP),研究不同工艺参数对放大反应的影响.结果表明,使用捏合机制备PAPP的工艺参数为反应温度260℃、反应时间5 h;该工艺下以热法磷酸制备的PAPP,w(P)为23.25%,w(N)为10.20%,pH为3.10,100 mL H2O中溶解度为1.12 g,1%热失重温度为303.34℃,以湿法磷酸为原料时制备的PAPP指标与之差异不大,均能满足团体标准T/CPCIF 0404-2024要求.将PAPP与聚磷酸三聚氰胺(MPP)复配添加至聚丙烯(PP)中,探究复配体系对PP阻燃性能的影响,结果表明,与空白样相比,PAPP(原料为湿法磷酸)添加量为15%、MPP添加量为10%时,复合材料的最大热释放速率和总热释放量分别降低了72.89%和11.84%;垂直燃烧测试通过1.6 mm V-0级别,极限氧指数由18.6%提升至35.4%,但拉伸强度下降了17.99%.
Abstract:
Piperazine pyrophosphate(PAPP)is synthesized using phosphoric acid and piperazine as raw materials via two-step process,and the effects of key process parameters on scale-up are systematically investigated.The results show that PAPP prepared from thermal method phosphoric acid under reaction temperature of 260℃and a reaction time of 5 h exhibits a phosphorus content of 23.25%,nitrogen content of 10.20%,pH of 3.10,solubility of 1.12 g in 100 mL H2O,and the 1%thermal weight loss temperature of 300.34℃.When prepared PAPP using wet-process phosphoric acid as the raw material,the indicators show little difference,and all can meet the requirements of the group standard T/CPCIF 0404-2024.PAPP is then blended with melamine polyphosphate(MPP)and incorporated into polypropylene(PP)to evaluate the flame-retardant performance of the composite system.Compared with the neat PP sample,the addition of 15%PAPP(derived from wet-process phosphoric acid)and 10%MPP reduces the peak heat release rate and total heat release by 72.89%and 11.84%,respectively.Moreover,the composite achieves a UL-94 V-0 rate at 1.6 mm thickness,and the limiting oxygen index is increased from 18.6%to 35.4%,however the tensile strength is decreased by 17.99%.
年,卷(期): 2026, 41(9)
分类号: TQ126.3+5
机标分类号: TQ325.14 TQ175.7 TQ420.6
在线出版日期: 2026年10月12日