军事知识服务平台
西昌钢钒1750m3高炉高球比条件下提钒钛矿比例技术攻关
De-bottling of increasing V-Ti ore ratio under high pellet ratio smelting at Xichang Steel & Vanadium 1750 m3 BF
摘要 为进一步降低生铁成本并提升铁水附加值,西昌钢钒炼铁厂开展在高球比条件下提钒钛矿比例技术攻关.通过选择合理的钒钛矿比例提高方式,采取强化原燃料质量保障、优化高炉操作制度等措施,实现高球比及高钒钛矿比例条件下的高效稳定生产.以3号高炉为例,炉料结构中全钒钛球团矿比例从52%左右提高至56%,钒钛矿比例从68.5%提高至71.3%,炉渣(TiO2)提高0.6个百分点,铁水[V]提高0.03个百分点;在入炉品位51.80%、炉渣(TiO2)为22.5%的条件下,利用系数达到2.71t/(m3·d),高炉工序能耗下降7kgce/t.
Abstract:
To cut hot metal cost and increase the added value of hot metal,the Ironmaking Plant of Xichang Steel & Vanadi-um launches a technical de-bottling campaign to increase the V-Ti ore ratio under high pellet ratio smelting.The measures include selecting a proper route for increasing the V-Ti ore ratio,enhancing quality management of raw material and fuel quality,and optimizing blast furnace operating system.Consequently,the furnace achieves efficient and stable production under high ratios of both pellet and V-Ti ore.Taking No.3 blast furnace as an example,the proportion of full V-Ti pellets in the burden mix rises from about 52%to 56%,that of V-Ti ore climbs from 68.5%to 71.3%,(TiO2)content of slag increases by 0.6%,and[V]content of hot metal heightens by 0.03%.Under conditions of ore grade of 51.80%and(TiO2)content of slag of 22.5%,the furnace productivity reaches 2.71 t/(m3·d),and the process energy intensity of the furnace lowers by 7 kgce/t.
刊 名 炼铁 PKU
年,卷(期): 2026, 45(4)
分类号: TF543
机标分类号: TF542.2 TF046.6 G64
在线出版日期: 2026年9月30日
基金项目: 2024ZD1003407:国家科技重大专项,