Technical breakthrough efforts and commercial test for extending tuyere life of Binxin Steel 1250 m3 BF
摘要
针对镔鑫钢铁1250m3高炉强化冶炼条件下风口寿命显著缩短问题,进行了延长风口寿命工业试验攻关.基于数值模拟结果,系统分析了风口破损机理,主要包括高温热负荷作用下的熔蚀、煤枪角度偏差导致的局部冲刷、冷却系统效能衰退引起的热积累,以及高温氧化与颗粒冲蚀的协同损伤.认为风口失效的本质是热-机械-化学多机制耦合作用的结果,在此基础上,提出了鼓风制度优化、喷煤比与富氧量调整、煤枪插入角度修正、加湿鼓风及冷却系统强化等一系列对策.试验结果显示,1、2号高炉风口寿命分别提升59.34%、76.85%,更换频率均显著下降,同时日产量稳定在5700~5800t/d,燃料比降至510~515kg/t.
Challenged by much shorter tuyere service life in Binxin Steel 1250 m3 blast furnace under intensified smelting con-dition,technical breakthrough efforts and commercial test are made for extending the tuyere life.It is systematically analyzed the tuyere damage mechanisms based on numerical simulation results,including melt loss under high-temperature thermal loads,local scouring caused by offset of pulverized coal injection(PCI)lance,heat accumulation due to declined cooling system efficiency,and damage resulted from co-action of high-temperature oxidation and particle erosion.The tuyere failure is believed caused by co-action of thermal,mechanical,and chemical mechanisms.Therefore,a series of countermeasures are taken,such as optimization of blasting system,adjustment of PCI rate and oxygen enrichment level,correction of PCI lance angles,application of humidified blast,and improvement of the cooling system.The test results show that tuyere serv-ice life of No.1 and No.2 BF increases by 59.34%and 76.85%respectively with replacement frequencies reduced signifi-cantly.Meanwhile,the furnace daily output stabilizes at 5700-5800t/d,and the fuel rate falls to 510-515 kg/t.