5×××系铝合金扁锭浇铸口表面黑斑缺陷的形成原因及改善措施
Causes and remedial measures for black spot defects on the surface of 5××× series aluminum alloy flat ingot spouts
摘要
为解决半连续直接水冷工艺生产5 ×××系铝合金扁锭浇铸口位置出现的区域性"黑斑"缺陷,通过宏观形貌观察、X射线衍射(XRD)物相分析、扫描电镜(SEM)及能谱(EDS)等方法对铸锭表面"黑斑"缺陷进行系统性研究.结果表明,该"黑斑"缺陷是MgO颗粒在铸造末期于浇铸口位置富集并凝固形成的.通过采用吊篮加镁技术、熔体覆盖保护、流槽加盖隔离等系列措施,可大幅减少"黑斑"缺陷,将铸锭探伤合格率由约75%提升至92%以上,镁元素回收率提升3.6%.
To address the localized"black spot"defects observed at the pouring spout of 5 ××× series aluminum alloy flat ingots produced via the semi-continuous direct water-cooling process,a systematic investigation of these surface defects was conducted using methods such as macroscopic morphol-ogy observation,X-ray diffraction(XRD)phase analysis,scanning electron microscopy(SEM),and energy-dispersive spectroscopy(EDS).The re-sults indicate that these"black spot"defects are formed by the accumulation and solidification of MgO particles at the pouring spout during the final stage of casting.By implementing a series of measures-including the use of a magnesium-loading basket,molten metal covering protection,and covering the flow channel to isolate the area-the"black spot"defects can be significantly reduced.This increased the non-destructive testing pass rate of ingots from approximately 75%to over 92%and boosted the magnesium recovery rate by 3.6%.
年,卷(期):
2026, (8)
分类号:
TF125+2
机标分类号:
TG146.2
TG335.5
TQ153
在线出版日期:
2026年10月23日