军事知识服务平台
35CrNiMo钢表面激光熔覆钴基合金涂层的微观组织及耐磨性能
Microstructure and Wear Resistance of Laser-Clad Cobalt-Base Alloy Coatings on 35CrNiMo Steel
摘要 采用激光熔覆技术在尺寸为100 mm×100 mm×10 mm的G35CrNiMo6-6 钢试样表面制备钴基合金涂层.通过摩擦磨损试验、金相检验和硬度测试研究了采用 2 200、2 500 和2 800 W激光功率以20、25 和30 mm/s 的扫描速率熔覆的涂层微观组织和耐磨性能.结果表明:涂层均由树枝晶和网状共晶组织组成,且随着激光功率和扫描速率的增加,枝晶均从柱状晶转变为等轴晶,共晶组织粗化;在1N载荷下摩擦磨损试验时涂层的磨损机制主要为磨粒磨损,而在30 N载荷下摩擦磨损试验时主要为磨粒磨损和氧化磨损;采用 2 800 W激光功率以25 mm/s的扫描速率熔覆的钴基合金涂层及组织为等轴枝晶和细小共晶的涂层均具有较好的耐磨性.
Abstract:
Cobalt-base alloy coatings were fabricated on G35CrNiMo6-6 steel specimens measuring 100 mm by 100 mm by 10 mm by a laser cladding technology.The microstructure and wear resistance of the coatings laser-clad with outputs of 2 200,2 500,and 2 800 W and at scanning rates of 20,25,and 30 mm/s were investigated via friction-wear testing,metallographic examination and hardness test.The results indicated that(a)the coatings all exhibited microstructure consisting of dendrites and eutectic network,as both the output and the scanning rare of laser increased,the dendrites all changed from columnar to equiaxed crystals,and the eutectic structure became coarser;(b)the wear mechanism of the coatings were primarily abrasive wear during friction-wear testing at load of 1 N,and abrasive wear and oxidative wear during friction-wear testing at load of 30 N;and(c)the cobalt-base alloy coating laser-clad with output of 2 800 W at scanning rate of 25 mm/s and the coating with microstructure consisting of equiaxed dendrites and fine eutectic crystal all possessed better wear performance.
刊 名 上海金属 ISTIC
年,卷(期): 2026, 48(5)
分类号: TG174.4 TG665
机标分类号: TG156.8+7 TG455 TG315.2
在线出版日期: 2026年9月30日
基金项目: 0703264:中国长江三峡集团有限公司资助项目,