Optimization of Composition of Electrolyte Used to Fabricate Low Roughness of Micro-arc Oxidation Film on Aluminum Alloy Vortex-Disc
摘要
涡旋压缩机的涡旋盘通常采用铝合金制作,需在电解液中进行微弧氧化处理,从而在其表面形成低粗糙度氧化膜.为了降低 4032 铝合金涡旋盘微弧氧化膜的表面粗糙度,对电解液成分进行优化,即采用六偏磷酸钠作主要成分,钨酸钠和四硼酸钠作辅料,并加入柠檬酸钠、EDTA二钠、丙三醇和氟化钠等添加剂.设计和进行了多组正交试验,对氧化膜粗糙度、厚度和硬度进行了加权综合评定.采用不同成分的电解液对 4032 铝合金试样进行微弧氧化处理,采用扫描电子显微镜检测氧化膜的微观形貌并进行能谱分析.结果表明:4032 铝合金试样微弧氧化膜的表面粗糙度(Ra)为0.485 μm,硬度为 783 HV0.2,厚度为 6.96 μm;电解液中四硼酸钠和氟化钠对氧化膜性能的影响最大,四硼酸钠能显著提高电解液的成膜性能,氟化钠能减少氧化膜表面的硬质颗粒.
Vortex-discs of vortex compressors are usually made from aluminum alloy,and require micro-arc oxidation treatment in an electrolyte,thus forming an oxidation film with low surface roughness.In order to reduce the surface roughness of the micro-arc oxidation film on 4032 aluminum alloy vortex-disc,the composition of electrolyte was optimized as follows:sodium hexametaphosphate as the primary component,sodium tungstate and sodium tetraborate as supplements,and additives including sodium citrate,disodium EDTA,glycerol,and sodium fluoride.The multiple sets of orthogonal experiments were designed and performed.The weighted comprehensive evaluation of roughness,thickness,and hardness of the oxide film was carried out.The micro-arc oxidation treatments of 4032 aluminum alloy specimens were performed in the electrolytes of different compositions,and the oxide film was tested for morphology by scanning electron microscope,and subjected to energy dispersive spectroscopy analysis.The results showed that(a)the micro-arc oxidation film on 4032 aluminum alloy specimen exhibited surface roughness(Ra)of 0.485 μm,hardness of 783 HV0.2,and thickness of 6.96 μm;(b)sodium tetraborate and sodium fluoride in the electrolyte had the most significant effect on the performance of the oxidation film,sodium tetraborate was able to considerably increase the film-forming capability of the electrolyte,and sodium fluoride was able to reduce the amount of hard particles on the oxide film.