军事知识服务平台
H13热作模具钢回火组织演变与力学性能调控
Microstructure Evolution and Mechanical Property Control of H13 Hot-work Die Steel during Tempering
摘要 以铸态H13热作模具钢为研究对象,采用1 100℃保温20 min油冷淬火后,分别在560、620、650℃下进行不同回火时间和回火次数的回火处理,利用OM、SEM、EPMA、XRD、EBSD及硬度、夏比冲击试验研究回火工艺对其组织演变和力学性能的影响.结果表明:回火温度是影响H13钢组织演变的主导因素.随着回火温度升高以及回火时间、次数增加,马氏体板条特征逐渐弱化,碳化物由细小弥散析出向聚集、球化和粗化转变,残余奥氏体含量和马氏体固溶碳含量总体降低,组织由回火马氏体向高温回火组织演变.560℃回火有利于保持较高硬度,其中,560℃回火65 min+回火三次组的硬度最高,为54.6HRC,但冲击吸收功较低;650℃回火可促进基体回复和碳化物球化,其中,650℃回火65 min+回火两次组的冲击吸收功最高,达到15.39 J,表现出了较好的冲击韧性.断口形貌由低温回火下的解理/准解理断裂逐渐向高温回火下的微孔聚集型韧性断裂转变.合理控制回火温度、回火时间和回火次数,可实现H13钢硬度与韧性的协同调控.
Abstract:
Taking as-cast H13 hot-work die steel as the research material,specimens were austenitized at 1 100℃for 20 min followed by oil quenching,and subsequently subjected to tempering treatments at 560℃,620℃and 650℃with varying tempering durations and cycles.Optical microscopy(OM),scanning electron microscopy(SEM),electron probe microanalysis(EPMA),X-ray diffraction(XRD),electron backscatter diffraction(EBSD),hardness measurements and Charpy impact tests were employed to investigate the effects of tempering parameters on microstructure evolution and me-chanical properties of the steel.The results reveal that tempering temperature dominates the microstructure evolution of H13 steel.With increasing tempering temperature,time and number of cycles,the lath feature of martensite gradually weakens;precipitated fine dispersed carbides undergo aggregation,spheroidization and coarsening,while the retained austenite content and dissolved carbon content in martensite show an overall decrease,and the microstructure evolves from tempered martensite to high-temperature tempered microstructure.Tempering at 560℃retains relatively high hardness,among which the group tempered at 560℃for 65 min with three cycles achieves the maximum hardness of 54.6 HRC,yet a low impact absorbed energy.Tempering at 650℃accelerates matrix recovery and carbide spheroidization,and the group tempered at 650℃for 65 min with two cycles achieves the highest impact absorbed energy of 15.39 J with superior impact toughness.The fracture morphology gradually transforms from cleavage/quasi-cleavage fracture at low tempering tempera-ture to dimple ductile fracture at high tempering temperature.Optimized regulation of tempering temperature,time and number of cycles enables synergistic improvement in hardness and toughness of H13 steel.
刊 名 特殊钢
年,卷(期): 2026, 47(5)
分类号: TG156.5
机标分类号: TG156.5 TG407 TB383
在线出版日期: 2026年9月21日
基金项目: U22A20173:国家自然科学基金,