军事知识服务平台
动力磷酸铁锂电池典型电性能及安全特性测试与研究
Test and research on typical electrical performance and safety characteristics of power lithium iron phosphate battery
摘要 以动力磷酸铁锂方形铝壳电池单体为研究对象,进行了在不同预紧力下容量和 DCR 测试,不同温度和不同荷电状态(SOC)下高倍率短时充放电测试,液冷快充循环测试,不同放电深度(DOD)和不同温度 100%DOD 循环寿命测试,以及不同位置挤压测试、极限热稳定性测试和过充电等安全测试.随着预紧力不断增大,可逆容量不断下降,DCR 逐渐升高.随着放电深度和测试温度的增加,容量保持率下降幅度越来越大,且容量保持率与循环次数在 25%~100%范围内近似成线性规律.随着环境温度的降低,放电倍率 Y 与荷电状态 X 的斜率值明显减小,以 50%SOC 为特定值进行线性拟合分析发现放电倍率 Y 与温度 θ 满足 Y=0.141θ+3.763 4(R2=0.995 6)线性关系方程,即温度每降低 10℃,其 30 s 放电电压控制在 2.50~2.55 V 目标值区间内所需的放电倍率约降低 1.25C.在相同 SOC 下,温度对低温高倍率放电的影响不再呈现线性规律,其中 0℃时短时高放电倍率仅相当于 10℃时放电倍率的 60%~69%,而-10℃时短时高放电倍率仅相当于 10℃时放电倍率的 40%~45%.经不同位置的挤压导致磷酸铁锂电池单体发生热失控的占比存在显著性差异,其中沿正、负极柱方向进行挤压发生热失控占比最高.在极限热稳定性测试中统计发现,磷酸铁锂方形铝壳电池单体开阀温度普遍在 140~150℃之间.温度达 300℃时电池单体仍未明显发生起火爆炸现象,均表现出优异的耐高温性能.钢针完全贯穿整个电池单体时,电池单体发生剧烈热失控,但整个过程中电池单体始终未起火及爆炸,表现出极其优异的安全性能.
Abstract:
Taking the cells of the lithium iron phosphate battery with square aluminum shell as the research object,tests were conducted under different pre-tightening forces for capacity and DCR measurement,high-rate short-time charge and discharge tests at different temperatures and different state of charge(SOC),liquid cooling fast charging cycle tests,100%SOC cycle life tests at different discharge depths(DOD)and different temperatures,as well as position compression tests,extreme thermal stability tests and overcharging safety tests.As the preload force continuously increases,the reversible capacity continuously decreases,and the DCR gradually rises.With the increase of discharge depth and test temperature,the decrease in capacity retention rate becomes more significant,and the capacity retention rate approximately follows a linear pattern with the number of cycles within the range of 25%to 100%.The capacity retention rate exhibits an approximately linear relationship with the number of cycles.As the ambient temperature decreases,the slope value of the discharge rate Y versus state of charge X decreases significantly.A linear fitting analysis was conducted with 50%SOC as the specific value,revealing a linear relationship between the discharge rate Y and temperature θ,which is expressed as Y=0.141θ+3.763 4(R²=0.995 6).In other words,for every 10℃drop in temperature,the discharge rate required to maintain the 30 s discharge voltage within the target range of 2.5~2.55 V decreases by approximately 1.25C.There are significant differences in the proportion of thermal runaway of lithium iron phosphate cell caused by extrusion at different positions.Among them,the proportion of thermal runaway caused by extrusion from the positive and negative pole directions is the highest.Statistical results in the ultimate thermal stability test show that the valve opening temperature of lithium iron phosphate prismatic cells is generally between 140~150℃,and no obvious fire or explosion occurs when the temperature reaches 300℃.When the steel needle completely penetrates the entire battery cells,the cells undergo a violent thermal runaway.However,throughout the entire process,the cells never caught fire or exploded,demonstrating extremely excellent safety performance.
刊 名 蓄电池
年,卷(期): 2026, 63(5)
分类号: TM912.2
机标分类号: TM912 TP393.08 U469.72
在线出版日期: 2026年9月30日