Study on the Swelling Inhibition and Seepage Promotion of Halloysite by Sucrose Complex Solution
摘要
采用原地浸出工艺开采中国南方某离子型稀土矿时,为抑制黏土矿物与稀土浸出液接触导致的水化膨胀,选用蔗糖与硫酸镁复配为抑膨浸出剂,考察了 0.01 mol/L~0.10 mol/L范围内不同浓度的蔗糖复配溶液对埃洛石黏土矿物膨胀行为和渗流行为的影响.结果表明,蔗糖复配硫酸镁溶液在浓度为0.02 mol/L时抑膨率最高,达到27.82%,稳定膨胀率为4.632%,对应的渗流速率为22.65×10-3 cm/min,抑膨效果最佳,且对渗流行为有一定的促进作用.由红外(FT-IR)、Zeta电位和热重分析(TG-DTA)结果可知,埃洛石黏土矿物与蔗糖复配浸出液充分接触时,蔗糖分子通过氢键的作用附着在黏土矿物的表面和层间,从而抑制了黏土矿物的膨胀行为.
When the ion-type rare earth ore in southern China is mined by in-situ leaching process,in order to restrain the hydration expansion caused by the contact between clay minerals and rare earth leaching solution,sucrose and magnesium sulfate were used as a compound swelling inhibitor.Effects of ten concentrations of sucrose(0.01 mol/L~0.10 mol/L)on the swelling behavior and percolation behavior of halloysite clay were investigated respectively.Experimental results show that the inhibition rate is the highest,reaching 27.82%,the stable swelling rate is 4.632%,the corresponding percolation rate is 22.65×10-3 cm/min under the concentration of sucrose and magnesium sulfate of 0.02 mol/L.This formulation not only dem-onstrates the most effective swelling suppression but also moderately enhances seepage behavior.According to FT-IR,Zeta po-tential and TG-DTA results,the sucrose molecules attach to the surface and interlayer of the clay minerals by hydrogen bonds when the complex solution of sucrose is in full contact with the clay minerals,the swelling rate of clay minerals is reduced.