碱熔—氟硅酸钾容量法测定传统陶瓷材料中二氧化硅
Determination of Silicon Dioxide in Traditional Ceramic Materials by Alkali Fusion-Potassium Fluorosilicate Volumetric Method
摘要
建立了碱熔-氟硅酸钾容量法测定传统陶瓷材料中二氧化硅的分析方法.优化了碱熔条件和氟硅酸钾沉淀工艺,加入过氧化氢消除钛离子干扰,以硝氮黄为指示剂,氢氧化钠标准溶液滴定.结果表明:在优化条件下,方法检出限为0.002 3 mg,定量限为0.007 7 mg;相对标准偏差(RSD,n=11)为0.076%;加标回收率为99.76%~100.04%.共存离子 Al3+、Fe3+、K+、Mg2+、Na+、Ti4+、Ba2+、Cu2+、Pb2+、Zn2+对测定无明显干扰.本法测定结果与国标法及第三方检测机构测定值相对偏差均<0.1%,适用于传统陶瓷材料中二氧化硅含量的测定.
An analytical method based on alkali fusion-potassium fluorosilicate volumetry was established for the determination of silicon dioxide in traditional ceramic materials.The alkali fusion conditions and potassium fluorosilicate precipitation procedures were optimized.Hydrogen peroxide was added to eliminate the interference of titanium ions,and sodium hydroxide standard solution was used for titration with nitrothiazole yellow as indicator.The results show that under optimized conditions,the limit of detection(LOD)of the method is 0.002 3 mg and the limit of quantitation(LOQ)is 0.007 7 mg;the relative standard deviation(RSD,n=11)is 0.076%;and the spiked recovery ranges from 99.76%to 100.04%.Coexisting ions including Al3+,Fe3+,K+,Mg2+,Na+,Ti4+,Ba2+,Cu2+,Pb2+and Zn2+have no obvious interference on the determination.The relative deviations between the measurement results obtained by this method and those from the national standard method and a third-party testing institution are all less than 0.1%.This method is suitable for the determination of silicon dioxide content in traditional ceramic materials.
年,卷(期):
2026, 55(4)
分类号:
O655.2
TQ174.1+8
机标分类号:
TQ127.2
O657.31
F203
在线出版日期:
2026年9月20日
基金项目:
51704104:国家自然科学基金,