摘要 本研究采用铝熔体原位反应法制备了Al-3Ti-4.35La中间合金,并借助XRD、OM、SEM和TEM等表征手段分析了x wt.%Al-3Ti-4.35La(x=0.1、0.2、0.3、0.4)中间合金添加量对Al-5Cu合金显微组织及力学性能的影响.结果表明,随着添加量的提升,晶粒尺寸表现为先减小后增大的趋势,力学性能呈现先增强后恶化的趋势.当添加0.3 wt.%Al-3Ti-4.35La中间合金后,可显著细化晶粒,晶粒由树枝晶向等轴晶转变,CuAl2 相由网状转变为短棒状及近球状.合金的抗拉强度、屈服强度、断后伸长率、显微硬度分别可达到184.86 MPa、88.93 MPa、13.45%和71.8 HV0.1,分别提升了28.40%、37.19%、258.67%和13.25%,力学性能得到显著改善.本研究为拓展Al-5Cu合金的工程化应用提供了理论支撑.
Abstract:
In this study,Al-3Ti-4.35La master alloy were prepared using the melt reaction method in molten aluminum.The effects of varying the addition of x wt.%Al-3Ti-4.35La(x=0.1,0.2,0.3,0.4)on the microstructure and mechanical properties of Al-5Cu alloys were analyzed using characterization techniques such as XRD,OM,SEM,and TEM.The results show that as the addition level increases,grain size first decreases and then increases,while mechanical properties first improve and then deteriorate.The addition of 0.3 wt.%Al-3Ti-4.35La master alloy significantly refines the grain structure,causing the grains to transform from dendritic to equiaxed,and the CuAl2 phase to change from a network-like structure to short rod-like and nearly spherical shapes.The alloy's tensile strength yield strength,elongation after fracture,and microhardness reached 184.86 MPa,88.93 MPa,13.45%,and 71.8 HV0.1,respectively,representing increases of 28.40%,47.19%,258.67%,and 13.25%,respectively,resulting in a significant improvement in mechanical properties.This study provides a theoretical foundation for expanding the engineering applications of Al-5Cu alloys.
刊 名 有色金属(中英文) ISTICPKU
年,卷(期): 2026, 16(10)
分类号: TG146.21
机标分类号: TG113.12 TG292 TG425
在线出版日期: 2026年10月28日