军事知识服务平台
La(NO3)3掺杂对Ti-10.5Mo-22Nb-6Zr MAO涂层显微硬度和耐蚀性的影响
The Influence of La(NO3)3 Doping on the Microhardness and Corrosion Resistance of Ti-10.5Mo-22Nb-6Zr MAO Coating
摘要 β-Ti钛合金因其优异的生物相容性、较低的弹性模量以及良好的力学性能,在生物医学植入材料领域展现出广阔的应用前景.其中,Ti-10.5Mo-22Nb-6Zr合金作为一种近β型钛合金,具有与人体骨骼相近的弹性模量,能够有效降低"应力屏蔽"效应,是目前骨科植入材料的理想选择之一.然而,该合金在实际应用过程中仍面临一些关键问题:其表面硬度较低,耐磨性能不足,在长期摩擦磨损条件下容易产生磨屑,引发炎症反应;同时,合金在生理环境中的耐腐蚀性能也有待提高,表面钝化膜的稳定性不足可能影响其服役寿命.因此,如何通过表面改性技术改善Ti-10.5Mo-22Nb-6Zr合金的耐磨性和耐蚀性,成为当前生物医用钛合金研究的重要课题.微弧氧化(Micro-arc oxidation,MAO)技术具有工艺简单、涂层与基体结合牢固、可大幅提高材料表面硬度等优点,已广泛应用于钛及钛合金的表面改性.稀土元素镧(La)具有较大的原子半径和较高的化学活性,能够在微弧氧化过程中参与涂层形成,细化晶粒、致密化涂层结构,有望同时提高涂层的耐磨性和耐蚀性.利用MAO技术在Ti-10.5Mo-22Nb-6Zr钛合金表面制备出陶瓷涂层,在优化后的微弧氧化基础电解液中引入稀土盐La(NO3)3,研究La(NO3)3 掺杂量对涂层形貌、耐磨性、润湿性和电化学性能的影响.利用SEM、显微硬度计、摩擦磨损试验机、润湿角测量仪、电化学工作站等对钛合金MAO涂层的表面形貌、显微硬度、摩擦因数、润湿角及电化学性能进行表征.研究结果表明:随着电解液中La(NO3)3 掺杂量增加,微弧氧化涂层表面孔洞逐渐减小,存在少量微裂纹,并附着有少量颗粒物.Ti-10.5Mo-22Nb-6Zr合金微弧氧化涂层的摩擦因数呈先减小后增加的趋势,最小值出现在试样M-4,即La(NO3)3 掺杂量为3 g·L-1 时,涂层耐磨性最佳.与未掺杂La(NO3)3 的试样对比,掺La(NO3)3 试样的显微硬度均有所提高.微弧氧化涂层显微硬度在3 g·L-1 时达到最大值,最大值约为(424.8±12.4)HV0.5.随着La(NO3)3 掺杂量增加,Ti-10.5Mo-22Nb-6Zr微弧氧化涂层的接触角呈现先减小后增加的趋势.Ti-10.5Mo-22Nb-6Zr钛合金微弧氧化涂层的极化曲线向正电位方向移动,腐蚀电位增加,腐蚀电流密度降低,降低幅度约为1~2个数量级.本研究旨在开发一种兼具优异耐磨性和耐蚀性的表面改性工艺,为该合金在生物医用领域的实际应用提供技术支撑.
Abstract:
β-Ti alloy showed broad application prospects in the field of biomedical implant materials due to its excellent biocompatibility,low elastic modulus and good mechanical properties.Among them,Ti-10.5Mo-22Nb-6Zr alloy,as a near β-titanium alloy,has an elastic modulus similar to that of human bones and can effectively reduce the"stress shielding"effect.It was one of the ideal choices for orthopedic implant materials.However,this alloy still faced some key problems in practical application:its surface hardness was relatively low and its wear resistance was insufficient.Under long-term friction and wear conditions,it was prone to generating wear debris and triggering inflammatory reactions.Meanwhile,the corrosion resistance of the alloy in physiological environments also needed to be improved and the insufficient stability of the surface passivation film may affect its service life.Therefore,how to improve the wear resistance and corrosion resistance of Ti-10.5Mo-22Nb-6Zr alloy through surface modification technology has become an important topic in the current research of biomedical titanium alloys.Micro-arc Oxidation(MAO)technology had the advantages of simple process,firm adhesion between coating and substrate and significant improvement of surface hardness of materials.It had been widely applied in the surface modification of titanium and titanium alloys.Lanthanum(La),a rare earth element,had a large atomic radius and high chemical reactivity.It can participate in coating formation during micro-arc oxidation,refine grains and densify the coating structure and was expected to simultaneously enhance the wear resistance and corrosion resistance of the coating.Ceramic coatings were prepared on the surface of self-made Ti-10.5Mo-22Nb-6Zr titanium alloy by using micro-arc oxidation(MAO)technology.Rare earth salt La(NO3)3 was introduced into the optimized micro-arc oxidation base electrolyte.The influence of the doping amount of La(NO3)3 on the morphology,wear resistance,wettability and electrochemical polarization curve of the coating was investigated.The surface morphology,microhardness,coefficient of friction,wetting angle and electrochemical performance of the MAO coating of near β-Ti alloy were characterized by SEM combined with energy dispersive spectrometer,microhardness tester,friction and wear testing machine,wetting angle measuring instrument and electrochemical workstation.The research results showed that as the doping amount of La(NO3)3 in the electrolyte increased,the pores on the surface of the micro-arc oxidation coating gradually decreased,there were a few micro-cracks on the coating surface and a small amount of particles adhered to the coating surface.The friction coefficient of the Ti-10.5Mo-22Nb-6Zr alloy micro-arc oxidation coating showed a trend of first decreasing and then increasing.The minimum value occurred in sample M-4,that is,when the doping amount of La(NO3)3 was 3 g·L-1,the wear resistance of the coating was the best.Compared with the samples without doping La(NO3)3,the microhardness of the samples doped with La(NO3)3 was all improved.The microhardness of the micro-arc oxidation coating reached its maximum value at 3 g·L-1,which was approximately(424.8±12.4)HV0.5.With the increase of the doping amount of La(NO3)3,the contact Angle of the Ti-10.5Mo-22Nb-6Zr micro-arc oxidation coating showed a trend of first decreasing and then increasing.The polarization curve of the Ti-10.5Mo-22Nb-6Zr titanium alloy micro-arc oxidation coating shifted towards the positive potential direction and the corrosion potential increased,so the corrosion current density decreased by approximately 1 to 2 orders of magnitude.This research aimed to develop a surface modification process that combines excellent wear resistance and corrosion resistance and can provide technical support for the practical application of this alloy in the biomedical field.
刊 名 有色金属(中英文) ISTICPKU
年,卷(期): 2026, 16(10)
分类号: TG174.4
机标分类号: TG174.4 R318.08 O643
在线出版日期: 2026年10月28日