军事知识服务平台
低钴锌浸出液中钴的富集及钴酸锂正极材料的制备
Cobalt enrichment from a cobalt-lean zinc leaching solution and preparation of LiCoO₂cathode material
摘要 针对湿法炼锌过程中锌液深度除钴及钴渣资源化利用的需求,本研究构建了锑盐深度净化除钴工艺体系,以实现锌液中钴的高效脱除与富集,并以富集钴渣为原料制备锂离子电池正极材料钴酸锂(LiCoO₂),开展了系统的工艺优化与材料性能研究.通过单因素试验系统考察了反应温度、反应时间、锌粉用量、溶液pH值等关键参数对除钴率的影响规律,优化得到锑盐深度净化除钴的最佳工艺条件:反应温度85℃、反应时间90 min、锌粉用量43 g/L、锑盐用量30 mg/L、溶液pH=4.0,该条件下除钴率可达99.53%,实现了锌液中钴的高效脱除与富集.在此基础上,以富集钴渣为原料,采用高温固相法制备LiCoO₂正极材料,通过XRD、SEM等表征手段分析其物相结构与微观形貌,并测试其电化学性能.结果表明,烧结温度与保温时间对LiCoO₂的结晶度具有显著调控作用,在焙烧温度800℃,时间8 h条件下目标物相完整形成,结晶度较好;制备所得LiCoO₂样品颗粒轮廓清晰,呈不规则块状,晶体结构完整;在1 C倍率下,材料充电容量达138.19 mAh/g,对应放电容量为132.55 mAh/g,首圈库伦效率达95.91%,展现出良好的充放电可逆性与电化学稳定性.本研究为湿法炼锌过程中钴的高效回收及锂电正极材料的低成本制备提供了可行的技术方案与理论支撑.
Abstract:
To address the industrial demands for deep cobalt removal from zinc electrolyte and resource utilization of cobalt residues in hydrometallurgical zinc production,this study established a technical system for deep purification and cobalt removal using antimony salt.The system enables efficient elimination and enrichment of cobalt from zinc electrolyte.Furthermore,systematic process optimization and material property investigations were carried out to prepare lithium cobalt oxide(LiCoO₂),a cathode material for lithium-ion batteries,from the cobalt-enriched residue.The effects of key parameters,including reaction temperature,reaction time,zinc powder dosage and solution pH,on cobalt removal efficiency were systematically investigated via single-factor experiments.The optimal process conditions for deep cobalt removal with antimony salt were determined as follows:reaction temperature of 85℃,reaction time of 90 min,zinc powder dosage of 43 g/L,antimony salt dosage 30 mg/L and solution pH of 4.0.Under these conditions,the cobalt removal rate reached 99.53%,realizing efficient elimination and enrichment of cobalt in zinc electrolyte.On this basis,LiCoO ₂ cathode material was synthesized from the cobalt-enriched residue via high-temperature solid-state reaction.Its phase structure and micromorphology were characterized by XRD and SEM,and its electrochemical performance was evaluated.The results demonstrate that calcination temperature and holding time exert a significant regulatory effect on the crystallinity of LiCoO₂,and under the conditions of temperature 800℃and time 8 h,the target phase was completely formed with good crystallinity.The as-prepared LiCoO₂ sample exhibits clear particle profiles,irregular blocky morphology and intact crystal structure.At a 1C rate,the material delivers a charge capacity of 138.19 mAh/g and a corresponding discharge capacity of 132.55 mAh/g,with an initial coulombic efficiency of 95.91%,showing excellent charge-discharge reversibility and electrochemical stability.This research provides a feasible technical scheme and theoretical support for the efficient recovery of cobalt in hydrometallurgical zinc processing and the low-cost preparation of lithium battery cathode materials.
刊 名 中国有色冶金 PKU
年,卷(期): 2026, 55(5)
分类号: TF813 TM912
机标分类号: TF813 O657.1 TD952.3
在线出版日期: 2026年11月6日
基金项目: 202411546009:广西大学生创新创业训练计划项目2023KY0881:广西高校中青年教师科研基础能力提升项目GXKS2024QNTD12:广西科技师范学院校级创团队S202511546048:广西大学生创新创业训练计划项目GXKS2022QN004:广西科技师范学院校级创团队GXKS2022QN005:广西科技师范学院科研项目,