摘要 针对新型Al-Cu-Mg-Ag合金在含Cl-腐蚀环境中易引发基体点蚀、晶间腐蚀等损伤等问题,本研究采用航空标准硫酸阳极氧化工艺在该铝合金表面形成致密氧化膜,并采用中性盐雾腐蚀试验、室温拉伸、轴向加载疲劳、扫描电镜、能谱等方法,分析表征膜层厚度、形貌、耐蚀性及合金力学性能,重点分析阳极氧化对合金高周疲劳性能及断裂机制的影响,得到以下主要结论.在150~200 g/L硫酸浓度范围内,膜层厚度先从4.6 µm缓慢增加至6.4 µm,再快速增加至10.2 µm,然后缓慢降低至10 µm,并且在200 g/L硫酸浓度,膜层出现粉化,推荐硫酸阳极氧化槽液中硫酸浓度为150~180 g/L;中性盐雾腐蚀试验考察了经硫酸阳极氧化标准工艺范围下限(13℃,13 V,20 min)、中限(19℃,17 V,40 min)、上限(26℃,22 V,60 min)所制备的样品,经336 h腐蚀后,三类样品表面光滑、平整,均表现出良好的耐蚀性;硫酸阳极氧化对合金室温拉伸性能无明显影响,但疲劳寿命降低约51%;未阳极氧化时,主疲劳裂纹源在试样轧制面萌生,扩展区面积较大;阳极氧化后,主裂纹源在试样棱角位置萌生,扩展区面积较小.
Abstract:
A novel Al-Cu-Mg-Ag alloy is susceptible to pitting and intergranular corrosion in Cl--containing environments.To address this,a dense anodic oxide film was fabricated on the alloy surface using an aviation-standard sulfuric acid anodizing process.Film thickness,morphology,corrosion resistance,and mechanical properties were evaluated by neutral salt spray testing,room-temperature tensile testing,axial-loading fatigue testing,scanning electron microscopy(SEM),and energy-dispersive spectroscopy(EDS),with emphasis on the effect of anodizing on high-cycle fatigue performance and fracture mechanism.Within a sulfuric acid concentration of 150~200 g/L,the film thickness increased gradually from 4.6 µm to 6.4 µm,then rapidly to 10.2 µm,before decreasing slightly to 10 µm.Powdering occurred at 200 g/L,and a concentration of 150~180 g/L is therefore recommended.Specimens prepared under the lower-limit(13℃,13 V,20 min),mid-limit(19℃,17 V,40 min),and upper-limit(26℃,22 V,60 min)conditions all retained smooth,intact surfaces after 336 h of neutral salt spray exposure,indicating good corrosion resistance.Anodizing exerted no significant influence on room-temperature tensile properties but reduced fatigue life by approximately 51%.Fractographic analysis showed that,in the non-anodized condition,the principal fatigue crack initiated at the rolled surface with a relatively large propagation region,whereas after anodizing the dominant crack originated at the specimen edge accompanied by a smaller propagation zone.
刊 名 中国有色冶金 PKU
年,卷(期): 2026, 55(5)
分类号: TG174.451 TG146
机标分类号: TG146.2 TF125.241 R363.2
在线出版日期: 2026年11月6日
基金项目: 2023YFB3710504:国家重点研发计划,